ASME SA213 / ASTM A213 316Ti UNS S31603 Stainless Steel Pipes

stars, based on 0reviews
5items available

ASME SA213 / ASTM A213 316Ti UNS S31603, EN 10216 - 5 1.4571 Stainless Steel Similar To Grade 316L Except That 316Ti Has Better High Temperature Strength, And Mechanical Strength. Used For Equipment Exposed To Aggressive Corrosive Conditions And High Temperature Applications,Including Automotive Flexible Connectors, Welded Bellows, Chimney Liners, And Flexible Ducting.
Type 316Ti Stainless Steel Is An Improved Corrosion Resistant Chrome-Nickel Steel Alloy With High Content Of Molybdenum And Some Titanium. It Is Not A Typical Free Machining Grade And Therefore Not Recommended For Difficult High Speed Machining Process.Grade 316Ti Stainless Steel Has Been Traditionally Specified By German Engineers And Users With The Werkstoff Number 316Ti.The Former Steel Grade In The UK Was 320S31.
316Ti Stainless Steel Is Essentially A Standard Carbon 316 Type With Titanium Stabilisation And Is Similar In Principle To The Titanium Stabilisation Of The 304 (1.4301) Type To Produce 321 (1.4541). The Addition Of Titanium Is Made To Reduce The Risk Of Intergranular Corrosion (IC) Following Heating In The Temperature Range 425-815C.The Addition Of Titanium Reduces The Risk Of IC Since Titanium Carbo-Nitrides Are Formed In Preference To Chromium Carbides Which Has The Effect Of Maintaining The Correct Distribution Of Chromium Throughout The Structure Of The Steel. 
The Weldability Of The 316Ti And 316L Can Be Assumed To Be Similar. Neither Of The Grades Can Be Expected To Weld 'Easier' Or 'Better' Than-The-Other. Niobium Stabilised Fillers (Welding Consumables) Should Be Used For Welding The 316Ti, Especially Where Elevated Temperature Weld Strength May Be Important. In Other Circumstances A '316L' Filler Should Give A Matching Weld Metal Aqueous Corrosion Resistance To That Of The 'Parent' '316Ti' Material.

316Ti SS Pipes - Industries & Applications

  • Gas Processing Industries

  • Petrochemical Industries

  • Power Generation Industries

  • Food Processing Industries

  • Chemical Industries

  • Oil & Gas Industries

  • Fertilizers Industries

  • Sugar Industries

316Ti SS Pipes Chemical Composition

Grade316Ti
minmax
C–0.08
Mn–2.0
Si–0.75
P–0.045
S–0.030
Cr16.018.0
Mo2.03.0
Ni10.014.0
N––


316Ti SS Pipes Mechanical Properties

Grade316Ti
Tensile Strength (MPa) min515
Yield Strength 0.2% Proof (MPa) min205
Elongation (% in 50mm) min35
HardnessRockwell B (HR B) max75
Rockwell B (HR B) max205


SS 316Ti Pipes Physical Properties

Grade316Ti
Density (kg/m3)8000
Elastic Modulus (GPa)193
Mean Coefficient of Thermal Expansion (m/m/0C)0-1000C17.2
0-3150C17.8
0-5380C18.4
Thermal Conductivity (W/m.K)at 1000C16.2
at 5000C21.5
Specific Heat 0-1000C (J/kg.K)500
Electrical Resistivity (n.m)720


SS 316Ti Pipes Equivalent Grades

Grade316Ti
UNS NoS31635
Old BritishBS320S31
EnX6CrNiMoTi17-12-2
EuronormNo1.4571
AFNORZ6CNDT17-12
GOST08Ch17N13M2T
Japanese JISSUS 316Ti