ASTM A333 GR. 6 22inch Diameter SCH80 Seamless Pipes 6-12.3m length

stars, based on 0reviews
7items available

ASTM A333 Low Temperature Service Carbon Steel Seamless Pipes


ASTM A333 (ASME S/A-333) Pipe grades permit low temperature service. This specification covers nominal (average) walled pipes including seamless and welded.  Several grades of ferritic steel are included. Some product sizes may not be available under this specification because heavier wall thicknesses have an adverse effect on low-temperature impact properties. A333 pipe is furnished to nine different grades designated by numbers 1, 3, 4, 6, 7, 8, 9, 10, & 11. 

Grade and Chemical Composition:

StandardGradeChemical Composition (%)
CSiMnPSCrNiCuMoVAl
ASTM A333Grade 1≤0.30
0.40~1.06≤0.025≤0.025





Grade 3≤0.190.18~0.370.31~0.64≤0.025≤0.025
3.18~3.82



Grade 4≤0.120.18~0.370.50~1.05≤0.025≤0.0250.44~1.010.47~0.980.40~0.75

0.04~0.30
Grade 6≤0.30≥0.100.29~1.06≤0.025≤0.025





Grade 7≤0.190.13~0.32≤0.90≤0.025≤0.025
2.03~2.57



Grade 8≤0.130.13~0.32≤0.90≤0.025≤0.025
8.40~9.60



Grade 9≤0.20
0.40~1.06≤0.025≤0.025
1.60~2.240.75~1.25


Grade 10≤0.200.10~0.351.15~1.50≤0.03≤0.015≤0.15≤0.25≤0.015≤0.50≤0.12≤0.06
Grade 11≤0.10≤0.35≤0.6≤0.025≤0.025≤0.5035.0~37.0
≤0.50

Mechanical Properities:

StandardGradeTensile Strength (MPa)Yield Point (MPa)Elongation (%)
YX
ASTM A333Grade 1≥380≥205≥35≥25
Grade 3≥450≥240≥30≥20
Grade 4≥415≥240≥30≥16.5
Grade 6≥415≥240≥30≥16.5
Grade 7≥450≥240≥30≥22
Grade 8≥690≥515≥22
Grade 9≥435≥315≥28
Grade 10≥550≥450≥22
Grade 11≥450≥240≥18

Strike Temperature Condition:

CradeThe lowest temperature for strike test
℉℃
Grade 1-50-45
Grade 3-150-100
Grade 4-150-100
Grade 6-50-45
Grade 7-100-75
Grade 8-320-195
Grade 9-100-75
Grade 10-75-60


ASTM A333 Grade 6 is the part of standard covers wall seamless and welded carbon and alloy steel pipe intended for use at low temperatures. ASTM A333 Grade 6 alloy pipe shall be made by the seamless or welding process with the addition of no filler metal in the welding operation.




Stockist, Suppliers and Exporter of ASTM A333 Gr 6, Low Temperature, pipe in China

  • Steel Grade : ASTM A333 Grade 6

  • Length : 5000 mm - 12000 mm or as per Client Requirement.

  • Outside Diameter : 1/2" to 24"

  • Wall Thickness : 2.00 mm to 100.00 mm

  • Delivery Terms : Max 1 week for Stock, 50 days for production.

 

My company hot sale alloy seamless tubes

Boiler tubes,( 20G. 12Cr1MoVG, ASTM A335 P5, P9, P11),

ASTM A333 GR.6 seamless pipes, ( 1” to 24” sch40, sch80, sch160),

 


Recent Reviews
+