Seamless Pipe EN10216
The standard is Seamless steel tubes for pressure purposesEN 10216-1: 2014 Seamless steel tubes for pressure purpo
Product Introduction
The standard is Seamless steel tubes for pressure purposes
EN 10216-1: 2014 Seamless steel tubes for pressure purposes. Technical delivery conditions. Non-alloy steel tubes with specified room temperature properties
EN 10216-2: 2014 Seamless steel tubes for pressure purposes. Technical delivery conditions. Non-alloy and alloy steel tubes with specified elevated temperature properties
EN 10216-3: 2014 Seamless steel tubes for pressure purposes. Technical delivery conditions. Alloy fine grain steel tubes
EN 10216-4: 2014 Seamless steel tubes for pressure purposes. Technical delivery conditions. Non-alloy and alloy steel tubes with specified low temperature properties
EN 10216-5: 2014 Seamless steel tubes for pressure purposes. Technical delivery conditions.
Stainless steel tubes
Seamless pipe production scope:
1” to 24” diameter, wallthickness: 3-40mm. Length 5-19m
Material: P195, P235, P265, P195GH, P235GH, P265GH, 13CrMo4-5, 10CrMo9-10

My company hot sale steel pipe and pipe fittings:
ASTM A106 B seamless pipes,(1” to 24” sch40, sch80),
API 5L GR.B steel pipes, (seamless pipe, LSAW pipe, SSAW pipes, 1” to 110” sch 40, sch80),
Boiler tubes,( 20G. 12Cr1MoVG, ASTM A335 P5, P9, P11),
ASTM A333 GR.6 seamless pipes, ( 1” to 24” sch40, sch80, sch160),
TP304/304L, TP316/TP316L, stainless steel pipes, (1” to 48” sch10, sch20, sch40, sch80),
API 5L X65, X70 PSL2 LSAW welded pipes, (20” to 60” sch40, sch80, sch160),
API 5CT seamless casing, and tubing, (2 3/8” to 20” K55, J55, N80, L80, P110),
Pipe fittings, elbow, reducer, ,tee,cap, flange
You Might Also Like
-

large diameter Seamless Line Pipes API 5L GR.B 1016x25.4 mm 6 m length
-

St37 Seamless Tube 88.9mm Diameter
-

Seamless Steel Pipe ASTM A106 B NACE MR 0175 12IN SCH160
-

Seamless Line Pipe API 5L GR.B 24INCH SCH40 12M Length
-

Seamless Pipe 2inch Idimeter XXS 6 M LENGTH Export
-

Seamless Pipe ASTM A106 C 10IN Diameter XS 12M Length