St37 Seamless Tube 88.9mm Diameter
St37 material seamless tube specification:OD:13 7mm-323 8mm WT:2mm-85mmLength:6
Product Introduction
DIN 1629 seamless pipes standard includes 3 basic steel grades (ST37, ST44, ST52.), this standard specifies the Seamless Circular Tubes of Non Alloys Steels that are used in construction of chemical plant, pressure vessels, pipe system and general mechanical and engineering purposes. Din 1629 seamless steel tubes and pipes are suitable for gas fusion welding, arc welding, flash butt welding, electric pressure welding and gas pressure welding.
DIN 1629 Steel Pipe Chemical Composition:
| Chemical Composition(%) | |||||
|---|---|---|---|---|---|
| Steel Grade | C | Si | Mn | P | S |
| St37 | ≤0.17 | - | - |
≤0.035
|
≤0.035 |
| St44 | ≤0.21 | - | - | ≤0.035 | ≤0.035 |
| St52.0 | ≤0.22 | ≤0.55 | ≤1.60 | ≤0.035 | ≤0.035 |
DIN 1629 Steel Pipe Mechanical Property:
| Mechanical Properties | ||||
|---|---|---|---|---|
| Steel Grade | Tensile strength(Mpa) | Yield point(Mpa) | Elongation(%)L | Elongation(%)T |
| St37 | 350-480 | ≥235 | ≥25 | ≥23 |
| St44 | 420-550 | ≥275 | ≥21 | ≥19 |
| St52.0 | 500-650 | ≥355 | ≥21 | ≥19 |
DIN 1629 Steel Pipe Equivalent Steel Grade:
| DIN 1629 | EN | BS NFA 49.210/49.112 | ASTM 53 |
|---|---|---|---|
| Grade St 37 | EN 10216.1Grade P235 T1 | Grade TU 37 B TU E 220 A | Grade A |
| Grade St 44 | EN 10216.1Grade P275T1 | Grade TU 42 B TU E 235 A | Grade B |
| Grade St 52-0 | EN 10216-3Grade P355N | NFA Grade P355N | ASME SA 381 Grade Y 52 |
Elevated Temperature Upper Yield Stress Values Of DIN 1629 Steel Pipe
| Steel Grade | Yield stress value by working temperature(Thickness increasing) | |||
|---|---|---|---|---|
| 50℃ | 200℃ | 250℃ | 300℃ | |
| St 37 | 235-215 | 185-170 | 165-150 | 140-130 |
| St 44 | 275-255 | 215-200 | 195-180 | 165-155 |
| St 52 | 355-335 | 248-230 | 225-210 | 195-185 |
-
St37 material seamless tube specification:
-
OD: 13.7mm-323.8mm
-
WT: 2mm-85mm
-
Length: 6m-12m or as required
-
Application: Pipeline steel pipe, vessel steel pipe, fluid pipe for low&medium pressure boiler
-
Supplementary Technology:
-
Tensile test, flattening test, leak tightness test, surface inspection, product analysis. Beveled end, plain end, varnished, or adding plastic caps as per customer’s requirements
-
Surface: Bared or painted, galvanized or with oiled or client option.
-
Delivery state: Hot Rolled, Cold Drawn
-
Steel Grade: St37, St44, St52


Galaxy Company Steel Pipe Product Hot Tags:
{seamless steel pipe| line pipe| boiler tube| ASTM A333 pipe| API 5L pipe| welded steel pipe| steel pipe inventory| steel plate,pipe fittings, Hot-dip galvanized welded pipe}
You Might Also Like
-

large diameter Seamless Line Pipes API 5L GR.B 1016x25.4 mm 6 m length
-

St37 Seamless Tube 88.9mm Diameter
-

Seamless Steel Pipe ASTM A106 B NACE MR 0175 12IN SCH160
-

Seamless Line Pipe API 5L GR.B 24INCH SCH40 12M Length
-

Seamless Pipe 2inch Idimeter XXS 6 M LENGTH Export
-

Seamless Pipe ASTM A106 C 10IN Diameter XS 12M Length
Send Inquiry