API 5L GR.B Seamless Pipe 20in SCH80 12m Length
API 5L Grade B pipe is a common grade pipe for oil and gas pipeline transmissions It also called L245 Pipe r
Product Introduction
API 5L Grade B pipe is a common grade pipe for oil and gas pipeline transmissions. It also called L245 Pipe refer ISO 3183, named by minimum yield strength 245 Mpa (355,000 Psi). Equivalent material ASTM A106 B or ASTM A53 B, which have similar value on chemical composition, mechanical properties, and applications.
API 5L Grade B Carbon Steel Seamless Pipe Chemical Composition
| Grade | Chemical Composition | |||||||
|---|---|---|---|---|---|---|---|---|
| C | Si | Mn | P | S | V | Nb | Ti | |
| API 5L Grade B PSL1 Pipe | 0.16 | 0.45 | 1.65 | 0.020 | 0.010 | 0.07 | 0.05 | 0.04 |
API 5L Grade B Pipe Suppliers Mechanical Properties
| Grade | Permissible yield point ratio | Yield Strength MPa(min) | Tensile Strength MPa | Elongation % (min) |
|---|---|---|---|---|
| API 5l Grade B Pipe | ≤ 0.85 | 245 | 415 | 23 |
Grade: API 5L Grade B Seamless Pipe
Outer Diameters: 1/2" - 30"
Thickness: SCH 20, SCH 40, SCH STD, SCH 80 To SCH 160
Range Of Length: SRL, DRL, 20FT, 40FT, 5 - 12 Meter
Product Specification Level: PSL1, PSL2, Sour Services
Ends: Plain, Beveled
Coatings: FBE, 3PE/3LPE, Black Painting, Varnished




My company hot sale steel pipe and pipe fittings:
ASTM A106 B seamless pipes,(1” to 24” sch40, sch80),
API 5L GR.B steel pipes, (seamless pipe, LSAW pipe, SSAW pipes, 1” to 110” sch 40, sch80),
Boiler tubes,( 20G. 12Cr1MoVG, ASTM A335 P5, P9, P11),
ASTM A333 GR.6 seamless pipes, ( 1” to 24” sch40, sch80, sch160),
TP304/304L, TP316/TP316L, stainless steel pipes, (1” to 48” sch10, sch20, sch40, sch80),
API 5L X65, X70 PSL2 LSAW welded pipes, (20” to 60” sch40, sch80, sch160),
API 5CT seamless casing, and tubing, (2 3/8” to 20” K55, J55, N80, L80, P110),
You Might Also Like
-

large diameter Seamless Line Pipes API 5L GR.B 1016x25.4 mm 6 m length
-

St37 Seamless Tube 88.9mm Diameter
-

Seamless Steel Pipe ASTM A106 B NACE MR 0175 12IN SCH160
-

Seamless Line Pipe API 5L GR.B 24INCH SCH40 12M Length
-

Seamless Pipe 2inch Idimeter XXS 6 M LENGTH Export
-

Seamless Pipe ASTM A106 C 10IN Diameter XS 12M Length
Send Inquiry