LSAW Line Pipe API 5L X60 PSL2 1219mmX38.1mm 12m Length
LSAW welded steel line pipe isproduced by double-side submerged arc welding and expanded diameter During the prod
Product Introduction
LSAW welded steel line pipe is produced by double-side submerged arc welding and expanded diameter. During the production used pre-welding and then precision welding process, it is stable welding process and high quality.
LSAW pipe applied to diameters from 18 in (457 mm) to 56 in (1524 mm), LSAW pipe also named as JCOE pipe by manufacturing procedures, forms in J Shape – C Shape – O Shape and E Cold Expansion.

| Product Name | LSAW Steel Pipe |
| Usage | Used for low pressure liquid delivery, such as water, gas, and oil. |
| Process | LSAW - UO(UOE),RB(RBE),JCO(JCOE) DSAW -Double Submerged arc welded |
| Standard | API 5L, API 5CT, ASTM 53, EN10217, DIN 2458. IS 3589, GB/T3091, GB/T9711 |
| Certificate | API 5L PSL1 / PSL2 |
| Out Diameter | 508mm- 1828.8mm |
| Wall Thickness | 10-70mm |
| Length | up to 12m,as request |
| Steel grade | API 5L PSL1 / PSL2,GR B, X42, X46, X52, X56, X60, X65, X70, X80 ASTM A53,GR A, GR B, GR C EN,S275, S275JR, S355JRH, S355J2H GB,Q195, Q215, Q235, Q345, L175, L210, L245, L320, L360- L555 |
| Surface | Fusion bond Epoxy coating, Coal Tar Epoxy, 3PE, Vanish Coating, Bitumen Coating, Black Oil coating as per customer's requirement |
| API 5L X60Q / X60N PSL 2 Chemical Composition | |||||||||
|---|---|---|---|---|---|---|---|---|---|
| Grade | Composition, % | ||||||||
| C | Si | Mn | P | S | V | Nb | Ti | Other | |
| X60N | 0.24 | 0.45 | 1.4 | 0.025 | 0.015 | 0.1 | 0.1 | 0.04 | g,h,l |
| X60Q | 0.18 | 0.45 | 1.7 | 0.025 | 0.015 | g | g | g | h,l |
| API 5L X60N / X60Q PSL 2 Mechanical Strength | ||||||
|---|---|---|---|---|---|---|
| Grade | Yield Strength Mpa | Tensile Strength Mpa | Raito | Elongation | ||
| Min | Max | Min | Max | Max | Min | |
| BN | 245 | 450 | 415 | 655 | 0.93 | F |
| BQ | ||||||
| X60N | 415 | 565 | 520 | 760 | 0.93 | F |
My Company Have Large Stocks Of API 5L X52, X60, X70 PSL2 LSAW Line Pipes. Delivery Is Very Fast.

My company hot sale steel pipe and pipe fittings:
ASTM A106 B seamless pipes,(1” to 24” sch40, sch80),
API 5L GR.B steel pipes, (seamless pipe, LSAW pipe, SSAW pipes, 1” to 110” sch 40, sch80),
Boiler tubes,( 20G. 12Cr1MoVG, ASTM A335 P5, P9, P11),
ASTM A333 GR.6 seamless pipes, ( 1” to 24” sch40, sch80, sch160),
TP304/304L, TP316/TP316L, stainless steel pipes, (1” to 48” sch10, sch20, sch40, sch80),
API 5L X65, X70 PSL2 LSAW welded pipes, (20” to 60” sch40, sch80, sch160),
API 5CT seamless casing, and tubing, (2 3/8” to 20” K55, J55, N80, L80, P110),
Pipe fittings, elbow, reducer, ,tee,cap, flange
You Might Also Like
-

large diameter Seamless Line Pipes API 5L GR.B 1016x25.4 mm 6 m length
-

St37 Seamless Tube 88.9mm Diameter
-

Seamless Steel Pipe ASTM A106 B NACE MR 0175 12IN SCH160
-

Seamless Line Pipe API 5L GR.B 24INCH SCH40 12M Length
-

Seamless Pipe 2inch Idimeter XXS 6 M LENGTH Export
-

Seamless Pipe ASTM A106 C 10IN Diameter XS 12M Length
Send Inquiry