Cangzhou Galaxy Steel Pipe Co., Ltd

banner
API 5CT Casing 7in 26ppf L80 R3 Range

API 5CT Casing 7in 26ppf L80 R3 Range

API 5CT L80 Casing Pipe DescriptionL80 steel casing pipe is a crucial tool utilized in oil well drilling (Other

Product Introduction

API 5CT L80 Casing Pipe Description

L80 steel casing pipe is a crucial tool utilized in oil well drilling (Other important tools consist of drill pipe, core barrel, casing, drill collar, little size steel tube used in drilling, etc.). This casing tube is made from steel of L80 grade. It is used for reinforcing the well wall. It is likewise a tunnel that provides petroleum from underground to surface area. This item is a completion tool used after the drilling procedure and in the past well cementation.

 Characteristic:

1. The thread and coupling of this steel casing pipe are specially processed which have smooth surface area without any burr, tear or other flaws. These defects might have a bad influence on the products’ strength and connection.

2. The mechanical homes of this product are greater than that of the J55 and K55 types. This steel casing pipe can be used to some more complicated development in much deeper holes. It can be used for the exploitation of middle-level oil and gas.

3. Due to the great efficiency of L80 material, this casing tube is extensively utilized in natural gas and coal bed methane extraction along with in geothermal wells.

4. The sizes of this pipes vary from 41/2″ to 20″. All pipes are produced strictly in accordance with API requirements.

Group Steel Grade Type Carbon Manganese Molybdenum Chromium

Nickel

Max.

Copper

Max.

Phosphorus

Max.

Sulfur

Max.

Silicon

Max.

Min. Max. Min. Max. Min. Max. Min. Max.
1 2 3 4 5 6 7 8 9 10 11 12 13 14 15 16
2 L80 1 – 0.43 – 1.9 – – – – 0.25 0.35 0.03 0.03 0.45
L80 9Cr – 0.15 0.3 0.6 0.9 1.1 8 10 0.5 0.25 0.02 0.01 1
L80 13Cr 0.15 0.22 0.25 1 – – 12 14 0.5 0.25 0.02 0.01 1
Any product is subject oil quenching process above, the upper limit of the carbon content of L80 steel grade can be increased to 0.50%.

API 5CT  L-80 SEAMLESS CASING AND TUBING SPECIFICATIONS

Readily available Sizes: 2 3/8 ″, 2 7/8 ″ and 3 1/2″ Outer Diameter
Grades: J55, K55, N80, L80, P110
Threading.
Heat treating.
External upset.
Hydrostatic Testing.
Full third-party examination capabilities (EMI, SEA, and Weld Line).
Couplings– EUE, AB Modified, denied, unique clearance couplings.
Finishing to client specifications.

End Finishing: External Upset Ends (EUE), PH6 (and equivalent connections), Flush Joint, Integral Joint (IJ). BTC,LB, SB