API 5CT K55 Casing 13-3/8" 68.00PPF LTC connection
API 5CT J55 casing is a seamless steel pipe applied in supporting the wall of petroleum and gas wells in order in order to ensure that the well is operating normally during and after the drilling process
Product Introduction
API 5CT J55 casing is a seamless steel pipe applied in supporting the wall of petroleum and gas wells in order to ensure that the well is operating normally during and after the drilling process. Each oil well will need several layers of casings depending on the different drilling depth and geological conditions. 5CT seamless casing has an excellent elongation property. After the casing is installed in the well, the well is be cemented. So seamless steel casing is not reusable. Therefore, casing pipe consumption will occupy more than 70% of the whole oil well pipes.
Properties: API 5CT casing tube is cooled after tempering process. This method can help the seamless casing avoid the high temperature brittleness and gain toughness, quenching method is adopted to reduce harmful elements and impurities effectively.
Applications: J55 casing pipe is widely used in the foundation works of many industries such as petroleum, natural gas, coal gas, water supply, thermal power generation, dredging engineering etc.
Features of API 5CT J55 Casing Tube
Strong, durable and reliable
J55 casing tube has sturdy construction
Economic rate of return is very high;
J55 casing tube is light in weight
Oil casing pipe is one of our main products. We will give you the products with competitive price in good quality:
Size: 4 1/2”-20”
Wall thickness: 0.224-0.514”
Grade: J55,K55,L80,N80,C90,T95,P110,Q125
Thread: STC,LTC,BTC
Length: API 5CT standard,R1,R2,R3
Package: Bundle or loose
Chemical Composition:
| Standard codes |
Models of steel tubes |
Chemical compositions(%) |
||||||||||
|
C |
Si |
Mn |
P |
S |
Cr |
Ni |
Cu |
Mo |
V |
Als |
||
|
API SPEC 5CT |
J55K55 (37Mn5) |
0.34~0.39 |
0.20~0.35 |
1.25~1.50 |
≤0.020 |
≤0.015 |
≤0.15 |
≤0.20 |
≤0.20 |
|
|
≤0.020 |
|
N80 (36 Mn2V) |
0.34~0.38 |
0.20~0.35 |
1.45~1.70 |
≤0.020 |
≤0.015 |
≤0.15 |
|
|
|
0.11~0.16 |
≤0.020 |
|
|
L80(13Cr) |
0.15~0.22 |
≤1.00 |
0.25~1.00 |
≤0.020 |
≤0.010 |
12.0~14.0 |
≤0.20 |
≤0.20 |
|
|
≤0.020 |
|
|
P110 (30CrMo) |
0.26~0.35 |
0.17~0.37 |
0.40~0.70 |
≤0.020 |
≤0.010 |
0.80~1.10 |
≤0.20 |
≤0.20 |
0.15~0.25 |
≤0.08 |
≤0.020 |
|
Mechanical Properties:
| Standard codes |
Models of steel tubes |
Tensite strength(MPa) |
Yield strength(MPa) |
Elongation(%) |
Hardness |
|
API SPEC 5CT |
J55 |
≥517 |
379~552 |
check the table |
|
|
K55 |
≥517 |
≥655 |
|
||
|
≥689 |
552~758 |
|
|||
|
≥655 |
552~655 |
≤241HB |
|||
|
P110 |
≥862 |
758~965 |
|


You Might Also Like
-

large diameter Seamless Line Pipes API 5L GR.B 1016x25.4 mm 6 m length
-

St37 Seamless Tube 88.9mm Diameter
-

Seamless Steel Pipe ASTM A106 B NACE MR 0175 12IN SCH160
-

Seamless Line Pipe API 5L GR.B 24INCH SCH40 12M Length
-

Seamless Pipe 2inch Idimeter XXS 6 M LENGTH Export
-

Seamless Pipe ASTM A106 C 10IN Diameter XS 12M Length
Send Inquiry