Seamless Steel Pipe Pile GB/T 8163 Q345B(ASTM A252 GR.3) 16" SCH160 12M LENGTH
Q345B 16Mn Seamless Structural Tube:Standard:GB 8162, GB T8163 ASTM A252 ASTM A53,ASTM A106(A,B),ASTM A500 A501 A519,JIS
Product Introduction
Q345B/16Mn Seamless Structural Tube:
Standard:
GB/8162, GB/T8163. ASTM A252/ASTM A53,ASTM A106(A,B),ASTM A500/A501/A519,JIS G3441/3444/3456,ISO2937, DIN 1626/17175
Grade:
Q345B,10#,20#,35#,45#;STPG 38,STS38,STB30,STB33,STB35,STPG42,,st37,st35.8,st35.4,st42,st45-8,st45-4
Pipe Application:
Used in general structure and mechanism such as construction, machinery, transportation, aviation, mining and each kind of structure tubes
|
Structure tube Outside diameter tolerance |
||
|
Hot rolled(extrude, expansion) |
±1% D or 0.50,choose the largest |
|
|
Cold drawn(rolled) |
±1% D or 0.30,choose the largest |
|
|
Cold drawn(rolled) structure tube Wall thickness Tolerance |
||
|
Steel pipe type |
Wall thickness |
Tolerances |
|
Cold Drawn(Rolled) |
<3 |
±15%,-10%S ,choose the larger one |
|
>3 |
±12.5%,-10%S |
|
Mechnical property for Q345B low alloy seamless structural steel tube:
| Thickness (mm) | ||||
| Q345B | ≤ 16 | > 16 ≤ 35 | > 35 ≤ 50 | >50 |
| Yield strength (≥Mpa) | 345 | 325 | 295 | 275 |
| Tensile strength (Mpa) | 470-630 | |||
►Chemical composition for Q345B low alloy structural steel (Heat Analysis Max%)
| Main chemical elements composition of Q345B | |||||||
| C | Si | Mn | P | S | V | Nb | Ti |
| 0.20 | 0.55 | 1.00-1.60 | 0.040 | 0.040 | 0.02-0.15 | 0.015-0.060 | 0.02-0.20 |
|
Steel Grade |
Tensile Strength Mpa |
Yield Strength Mpa |
Elongation% |
||
|
<16 |
16-30 |
>30 |
|||
|
MIN |
|||||
|
10# |
335- |
205 |
195 |
1185 |
24 |
|
20# |
390 |
245 |
235 |
225 |
20 |
|
35# |
510 |
305 |
295 |
285 |
17 |
|
45# |
590 |
335 |
325 |
315 |
14 |
|
Structure tube chemical compositon |
|||||||||
|
Standard
|
Grade
|
C |
Si |
Mn |
P< |
S< |
Cu< |
Ni< |
Cr< |
|
GB/T8162 |
10# |
0.07-0.14 |
0.17-0.37 |
0.35-0.65 |
0.035 |
0.035 |
0.25 |
0.25 |
0.15 |
|
20# |
0.17-0.24 |
0.17-0.37 |
0.35-0.65 |
0.035 |
0.035 |
0.25 |
0.25 |
0.25 |
|
|
35# |
0.32-0.39 |
0.17-0.37 |
0.50-0.80 |
0.035 |
0.035 |
0.25 |
0.25 |
0.25 |
|
|
45# |
0.42-0.50 |
0.17-0.37 |
0.50-0.80 |
0.035 |
0.035 |
0.25 |
0.25 |
0.25 |
|
1.Size: from 1/2" to 36"
2.Wall Thickness: From 2mm to 60mm
3.Schedule: Sch20,Sch 30,SCH40, STD, SCH80,...SCH160
4.Length: 5.8 meters for 20' container, 6 meters to 12 meters for 40' container, or acc. to clients' requirement
5.Packing: aac. to clients' requirement
8.Surface finishing: Varnish coating, bevelled ends with caps
9.Third party inspection: BV, SGS, Lloyds etc.
10.Supply Ability: 1900MT/month
11.Standard:API 5L/5CT, ASTM A106,A53 ,DIN ,EN ,JIS,BS and equivalent
12.Material: GR.B,20#,Q345, ST45,ST35.8 ,ST52,X42,X52,X60...
13. We have these seamless pipe stock about 4000tons. delivery is very fast.


My company hot sale seamless steel line pipes:
ASTM A106 B seamless pipes, API 5L GR.B seamless steel pipes(1” to 24” sch40, sch80),
API 5L X52, X65, X70 PSL2 seamless line pipe (2” to 24” sch40, sch80, sch160),
You Might Also Like
-

large diameter Seamless Line Pipes API 5L GR.B 1016x25.4 mm 6 m length
-

St37 Seamless Tube 88.9mm Diameter
-

Seamless Steel Pipe ASTM A106 B NACE MR 0175 12IN SCH160
-

Seamless Line Pipe API 5L GR.B 24INCH SCH40 12M Length
-

Seamless Pipe 2inch Idimeter XXS 6 M LENGTH Export
-

Seamless Pipe ASTM A106 C 10IN Diameter XS 12M Length
Send Inquiry