Carbon Steel Seamless Pipes GB/T8163 Q345E SIZE: 60.3-1016mm 6m and 12m length
Seamless steel pipe with GB T8162 Q345C lower tempreatureQ345 steel pipehave good comprehensive mechanical properties
Product Introduction
Seamless steel pipe with GB/T8163 Q345C lower tempreature
Q345 steel pipe have good comprehensive mechanical properties,Low Temperature performance can also,Plasticity and weldability is good, apply to the low pressure vessel, oil tank, vehicles, cranes, mining machinery, power stations, Bridges,Can be used in various structure below 40 ℃ cold areas.
Q345A Chemical composition
C≤0.20 Mn 1.0~1.6 Si≤0.55 P≤0.045 S≤0.045 V 0.02~0.15
Tensile strength(mpa):490-675
proof stress(mpa):≥345
Elongation(%):≥21
Q345B Chemical composition
C≤0.20 Mn 1.0~1.6 Si≤0.55 P≤0.040 S≤0.040 V 0.02~0.15
Tensile strength(mpa):490-675
proof stress(mpa):≥345
Elongation(%):≥21
Q345C Chemical composition
C≤0.20 Mn 1.0~1.6 Si≤0.55 P≤0.035 S≤0.035 V 0.02~0.15 Al≥0.015
Tensile strength(mpa):490-675
proof stress(mpa):≥345
Elongation(%):≥21
Q345D Chemical composition
C≤0.18 Mn 1.0~1.6 Si≤0.55 P≤0.030 S≤0.030 V 0.02~0.15 Al≥0.015
Tensile strength(mpa):490-675
proof stress(mpa):≥345
Elongation(%):≥22
Q345E Chemical composition
C≤0.18 Mn 1.0~1.6 Si≤0.55 P≤0.025 S≤0.025 V 0.02~0.15 Al≥0.015
Tensile strength(mpa):490-675
proof stress(mpa):≥345
Elongation(%):≥22
Q345A,Q345B,Q345C,Q345D,Q345E
Their impact of temperature is different
Q345A--- Do not impact
Q345B---20 degrees temperature impact
Q345C---Zero impact
Q345D--- - 20 degrees impact
Q345E--- - 40 degrees impact
Specification:
1. Out Diameter: 21.3mm - 800mm
2. Thickness: 0.6mm -120.0mm
3. Steel Grade: Q195-Q345, 10#-45#, ST35,ST45,ST52, 1010,1045,4130,4140
4. Standard: GB/T 3091-2001, BS1387-1985, DIN EN10025, EN10219, ASTM SCH40, ASTM SCH80
5. Surface Finish: Galvanized, electro galvanized, black
6.Length: 5-15m maximum
7. Process Method: HOT ROLLED or HOT EXPANSION
8.Pipe Ends: Square cut or bevelled
Package: Suitable packing according to the size of the pipes.
Supply Ability: 3000 metric tons per month.
My company has many STOCK of Q345 seamless pipes. about 15000tons, the pipes is from TPCO, ANGANG, BAOSTEEL, Baotou melong, Fengbao etc.
Exports to Europe, North America, the Middle East, Africa, Asia and other countries and regions.



Galaxy Company Hot Sale Steel Pipe Products:
OCTG, casing, tubing, seamless steel pipe, line pipe, boiler tube, ASTM A333 pipe, ASTM A335 alloy pipes, Mechanical pipe, API 5L pipe,
You Might Also Like
-

large diameter Seamless Line Pipes API 5L GR.B 1016x25.4 mm 6 m length
-

St37 Seamless Tube 88.9mm Diameter
-

Seamless Steel Pipe ASTM A106 B NACE MR 0175 12IN SCH160
-

Seamless Line Pipe API 5L GR.B 24INCH SCH40 12M Length
-

Seamless Pipe 2inch Idimeter XXS 6 M LENGTH Export
-

Seamless Pipe ASTM A106 C 10IN Diameter XS 12M Length
Send Inquiry