Stainless Steel Tubing For Heat Exchanger 19.05X1.5MM TP316L
Specification of Stainless Steel tube for heat exchangerOuter Diameter :6 35 mm OD to 114mm ODThickness :0 70 mm
Product Introduction
Specification of Stainless Steel tube for heat exchanger
Outer Diameter : 6.35 mm OD to 114mm OD
Thickness : 0.70 mm to 12.70 mm, SCH10S,SCH40S,SCH80S,SCH160S
Technique: Seamless (Cold Drawn/Cold Rolling), Welded
Material: TP304,TP304L,TP304H,TP316, TP316L,TP316Ti, TP309,TP310S,TP314, TP317L, TP321, TP347H,904L, S31803,S32205, S32750 etc.
Length : up to 12 Meters Leg Length & Customed Length
Standard : ASTM A688 / ASTM SA688 / ASTM A249 / ASTM A789/ ASTM A213, JIS 3463 and JIS 3459, DIN 2462, DIN 17458 and DIN 17456, GOST 9941
Finish: Annealed, pickled & polished, BA
Stainless Steel Tubes Size for Heat Exchanger
| Outside Diameter | |||||||||
| 25 | 22 | 20 | 18 | 16 | 14 | 12 | 10 | ||
| Wall Thickness mm | |||||||||
| 0.508 | 0.71 | 0.89 | 1.24 | 1.65 | 2.11 | 2.77 | 3.40 | ||
| mm | inch | Weight kg/m | |||||||
| 6.35 | 1/4 | 0.081 | 0.109 | 0.133 | 0.174 | 0.212 | |||
| 9.53 | 3/8 | 0.126 | 0.157 | 0.193 | 0.257 | 0.356 | 0.429 | ||
| 12.7 | 1/2 | 0.214 | 0.263 | 0.356 | 0.457 | 0.612 | 0.754 | ||
| 15.88 | 5/8 | 0.271 | 0.334 | 0.455 | 0.588 | 0.796 | 0.995 | ||
| 19.05 | 3/4 | 0.327 | 0.405 | 0.553 | 0.729 | 0.895 | 1.236 | ||
| 25.4 | 1 | 0.44 | 0.546 | 0.75 | 0.981 | 1.234 | 1.574 | 2.05 | |
| 31.75 | 1 1/4 | 0.554 | 0.688 | 0.947 | 1.244 | 1.574 | 2.014 | 2.641 | |
| 38.1 | 1 1/2 | 0.667 | 0.832 | 1.144 | 1.514 | 1.904 | 2.454 | 3.233 | |
| 44.5 | 1 3/4 | 1.342 | 1.774 | 2.244 | 2.894 | 3.5 | |||
| 50.8 | 2 | 1.549 | 2.034 | 2.574 | 3.334 | 4.03 | |||
| 63.5 | 2 1/2 | 1.949 | 2.554 | 3.244 | 4.214 | 5.13 | |||
| 76.2 | 3 | 2.345 | 3.084 | 3.914 | 5.094 | 6.19 | |||
| 88.9 | 3 1/2 | 2.729 | 3.609 | 4.584 | 5.974 | 7.27 | |||
| 101.6 | 4 | 4.134 | 5.254 | 6.854 | 8.35 | ||||
| 114.3 | 4 1/2 | 4.654 | 5.924 | 7.734 | 9.43 |
||||



My company hot sale stainless steel pipe:
TP304/304L, TP316/TP316L, TP347, stainless steel welded Pipes, stainless seamless pipes, stainless steel welded and seamless pipes, (1” to 48” sch10, sch20, sch40, sch80)
You Might Also Like
-

large diameter Seamless Line Pipes API 5L GR.B 1016x25.4 mm 6 m length
-

St37 Seamless Tube 88.9mm Diameter
-

Seamless Steel Pipe ASTM A106 B NACE MR 0175 12IN SCH160
-

Seamless Line Pipe API 5L GR.B 24INCH SCH40 12M Length
-

Seamless Pipe 2inch Idimeter XXS 6 M LENGTH Export
-

Seamless Pipe ASTM A106 C 10IN Diameter XS 12M Length
Send Inquiry