SUS TP316Ti Stainless Steel Seamless Pipe 12in SCH160
316Ti STAINLESS STEEL PIPE BRIEF INTRODUCTION316Ti stainless steel pipeis a hollow long round steel pipe which is
Product Introduction
316Ti STAINLESS STEEL PIPE BRIEF INTRODUCTION
316Ti stainless steel pipe is a hollow long round steel pipe which is widely used in petroleum, chemical, medical, food, light industry, machinery, instrument and other industrial pipeline and mechanical structure parts, etc. In addition with in bending and torsion strength, the weight is lighter, so it is also widely used to make mechanical parts and engineering structures. It is also used to produce all kinds of conventional weapons, guns and shells.
Chemical Composition of ASTM A312 / A213 SS TP316Ti Pipe and Tube
| Grade | C | Mn | Si | P | S | Cr | Mo | Ni | Fe |
| SS TP 316Ti | 0.08 max | 2.0 max | 0.75 max | 0.045 max | 0.030 max | 16.00 – 18.00 | 2.00 – 3.00 | 10.00 – 14.00 | 68.395 min |
Mechanical Property of Stainless Steel UNS S31635 Pipes and Tubing
| Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| 8.0 g/cm3 | 1399 °C (2550 °F) | Psi – 75000 , MPa – 515 | Psi – 30000 , MPa – 205 | 35 % |
316Ti Stainless Steel Pipes and Tubing Equivalent Grades
| Grade | North America | France | Germany | European | Japan | Russia | European | Italy | Sweden | UK | USA |
| UNS | AFNOR | DIN | W.N. | JIS | GOST | EN | UNI | SIS | BS | AISI | |
| SS 316Ti | S31635 | Z 2 CND 17-13-Az | X 5 CrNiMo 17 13 3 | 1.4571 | – | 08KH16N13M2B | X 3 CrNiMo 17 13 3 | X 2 CrNiMo 1713 | 23 53 | 316S13 | 316Ti |
Size (Seamless) : 1/2″ NB – 16″ NB
Size (ERW) : 1/2″ NB – 24″ NB
Size (EFW) : 6″ NB – 100″ NB
Outside Diameter : 6.00 mm OD up to 914.4 mm OD, Sizes up to 24” NB available Ex-stock, OD Size Steel Tubes available Ex-stock
Thickness Range : 0.3mm – 80 mm, SCH 5, SCH10, SCH 40, SCH 80, SCH 80S, SCH 160, SCH XXS, SCH XS
Length : Single Random, Double Random & Required Length End: Plain End, Beveled End, Treaded
Type : Seamless, ERW, Welded, Fabricated, CDW
Form : SS 316Ti Round Pipes/Tubes, SS 316Ti Square Pipes/Tubes, SS 316Ti Rectangular Pipe/Tubes, SS 316Ti Coiled Tubes, SS 316Ti “U” Shape, SS 316Ti Pan Cake Coils, SS 316Ti Hydraulic Tubes
Inspection, Test Reports : Mill Test Certificates, EN 10204 3.1, Chemical Reports, Mechanical Reports, PMI Test Reports, Visual Inspection Reports, Third Party Inspection Reports, NABL Approved Lab Reports, Destructive Test Report, Non Destructive Test Reports
Delivery Condition : Annealed and Pickled, Polished, Bright Annealed, Cold Drawn
My company hot sale stainless steel pipe:
TP304/304L, TP316/TP316L, TP347, stainless steel welded Pipes, stainless seamless pipes, stainless steel welded and seamless pipes, (1” to 48” sch10, sch20, sch40, sch80),TP321, TP347 stainless steel seamless pipes, (1/2”to 24” seamless

You Might Also Like
-

large diameter Seamless Line Pipes API 5L GR.B 1016x25.4 mm 6 m length
-

St37 Seamless Tube 88.9mm Diameter
-

Seamless Steel Pipe ASTM A106 B NACE MR 0175 12IN SCH160
-

Seamless Line Pipe API 5L GR.B 24INCH SCH40 12M Length
-

Seamless Pipe 2inch Idimeter XXS 6 M LENGTH Export
-

Seamless Pipe ASTM A106 C 10IN Diameter XS 12M Length
Send Inquiry