Stainless Pipe A312 GR.TP304L,EFW,PE,36.19,SCH.10S 18inX9.53 12m Length
ASTM A312 312M standardThis specificationcovers seamless, straight-seam welded, and heavily cold worked welded austeni
Product Introduction
ASTM A312/312M standard
This specification covers seamless, straight-seam welded, and heavily cold worked welded austenitic stainless steel pipe intended for high-temperature and general corrosive service.
Main Steel Grades - TP 304, TP 304L, TP 316, TP 321
|
Chemical Composition (%, max) |
||||||||
|
Steel Grade |
C |
Si |
Mn |
Cr |
Ni |
Mo |
S |
P |
|
TP304 |
0,08 |
0,75 |
2 |
18 - 20 |
8 - 11 |
- |
0,03 |
0,04 |
|
TP304L |
0,035 |
0,75 |
2 |
18 - 20 |
8 - 13 |
- |
0,03 |
0,04 |
|
TP316 |
0,08 |
0,75 |
2 |
16 - 18 |
11 - 14 |
2 - 3 |
0,03 |
0,04 |
|
TP316L |
0,035 |
0,75 |
2 |
16 - 18 |
10 - 15 |
2 - 3 |
0,03 |
0,04 |
|
TP321 |
0,08 |
0,75 |
2 |
17 - 20 |
9 - 13 |
- |
0,03 |
0,04 |
|
Mechanical properties
|
|||
|
Steel Grade |
Tensile Strength, N/mm2 (min) |
Yield Strength, N/mm2 (min) |
Elongation, % (min) |
|
TP304 |
515 |
205 |
35 |
|
TP304L |
485 |
170 |
35 |
|
TP316 |
515 |
205 |
35 |
|
TP316L |
485 |
170 |
35 |
|
TP321 |
OD < 17,1 mm - 515; |
OD < 17,1 mm - 205; |
35 |
ASTM A213 TP 304L stainless pipe
TP304L Stainless Steel Pipe is widely used in petroleum, chemical, medical, food, light industry, machinery, instrument and other industrial pipeline and mechanical structure parts, etc. In addition, in bending and torsion strength, the weight is lighter, so it is also widely used to make mechanical parts and engineering structures.


My company hot sale stainless steel pipe:
TP304/304L, TP316/TP316L, TP347, stainless steel welded Pipes, stainless seamless pipes, stainless steel welded and seamless pipes, (1” to 48” sch10, sch20, sch40, sch80),
TP321, TP347 stainless steel seamless pipes, (1/2”to 24” seamless)
You Might Also Like
-

large diameter Seamless Line Pipes API 5L GR.B 1016x25.4 mm 6 m length
-

St37 Seamless Tube 88.9mm Diameter
-

Seamless Steel Pipe ASTM A106 B NACE MR 0175 12IN SCH160
-

Seamless Line Pipe API 5L GR.B 24INCH SCH40 12M Length
-

Seamless Pipe 2inch Idimeter XXS 6 M LENGTH Export
-

Seamless Pipe ASTM A106 C 10IN Diameter XS 12M Length
Send Inquiry