321 Stainless Steel pipes 12" SCH80
321 stainless steel (UNS S32100) is a titanium stabilized austenitic stainless steel that features improved resistance to intergranular corrosion This grade is suitable for high-temperature applications up to 1500°F (815°C)
Product Introduction
321 stainless steel (UNS S32100) is a titanium stabilized austenitic stainless steel that features improved resistance to intergranular corrosion. This grade is suitable for high-temperature applications up to 1500°F (815°C), where the addition of titanium stabilizes the material against chromium carbide formation. Since titanium has a stronger affinity for carbon than chromium, titanium carbide precipitates within the grain instead of forming at the grain boundaries. While corrosion resistance is similar to 304 and 304L in the annealed condition, it features higher creep and stress rupture properties. These properties make it ideal for pressure vessels and boiler applications. 321 stainless steel is non-magnetic and heat resistant for continuous service at elevated temperatures.
Alloy 321 stainless steel plate is also advantageous for high temperature service because of its good mechanical properties. Alloy 321 stainless steel plate offers higher creep and stress rupture properties than Alloy 304 and, particularly, Alloy 304L, which might also be considered for exposures where sensitization and intergranular corrosion are concerns.
Alloy 321 stainless steel plate cannot be hardened by heat treatment, only by cold working. It can be easily welded and processed by standard shop fabrication practices.
Standards:
ASTM 321/321H Sheets
UNS S32100/S32109 Sheets
EN number 1.4541* Sheets
EN name * 6CrNiTi18-10*
W.Nr. 1.4541/1.4878 Sheets
DIN *6 CrNiTi 18 10/ 12CrNiTi18 9 Sheets
SS 2337 Sheets
SS 321 Chemical Composition
|
SS Grade |
C |
Si |
Mn |
P |
S |
Cr |
Mo |
Ni |
N |
Other |
|
|
Type 321 |
min. |
- |
00.75 |
2.00 |
00.045 |
00.030 |
17.0 |
- |
9.0 |
00.10 |
Ti=5(C+N) |
|
Type 321H |
min. |
00.04 |
00.75 |
2.00 |
00.045 |
00.030 |
17.0 |
- |
9.0 |
- |
Ti=4(C+N) |
|
Type 347 |
min. |
00.08 |
00.75 |
2.00 |
00.045 |
00.030 |
17.0 |
- |
9.0 |
- |
Nb=10(C+N) |
Stainless Steel 321 Mechanical Properties



|
SS Type |
Tensile Strength minimum (MPa) |
Yield Strength 0.2% Proof minimum (MPa) |
Elongation minimum (% in 50mm) |
Hardness |
|||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
|
Rockwell B (HR B) maximum |
Brinell (HB) maximum |
||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
|
321 |
515 |
205 |
40 |
95 |
217 |
||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
|
321H |
515 |
205 |
40 |
95 |
217 |
||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
|
347 |
515 |
205 |
40 |
92 |
201 Alloy 321 stainless steel plate cannot be hardened by heat treatment, only by cold working. It can be easily welded and processed by standard shop fabrication practices. SS 321 Chemical Composition
Stainless Steel 321 Mechanical Properties
|
||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
You Might Also Like
-

large diameter Seamless Line Pipes API 5L GR.B 1016x25.4 mm 6 m length
-

St37 Seamless Tube 88.9mm Diameter
-

Seamless Steel Pipe ASTM A106 B NACE MR 0175 12IN SCH160
-

Seamless Line Pipe API 5L GR.B 24INCH SCH40 12M Length
-

Seamless Pipe 2inch Idimeter XXS 6 M LENGTH Export
-

Seamless Pipe ASTM A106 C 10IN Diameter XS 12M Length
Send Inquiry