12Cr1MoVG boiler steel pipe 20" sch100 size
GB 5310 12Cr1MoVG High Pressure Boiler Tubes, Seamless steel tubes and pipes for high pressure boiler GB 5310 standard is applicable to steam boilers for high pressure 12Cr1MoVG boiler steel pipe is used for high-pressure boilers heating surface tubes
Product Introduction
Standard: GB/T 5310
Equivalent Standards: EN 10216-2, ASTM A369, BS 3059 Part I, NF A 49-213, DIN 17175, JIS G3458, JIS G3461, JIS G3462, ASTM A213, ASTM A335, EN 10216-5, JIS G3463, JIS G3459, ASTM A210, ASTM A106, ASTM A178
Material: 12Cr1MoVG
Equivalent Materials: 1Cr-0.5Mo-V
Manufacture: tubes to GB/T 5310 shall be manufactured by hot rolled or cold drawn.
Heat Treatment: the tubes shall be produced by heat treated, WT≤30mm normalizing & tempering, WT>30mm quenching & tempering.
Length: 4000mm; 6000mm; 9000mm; 12000mm; and so on.
12Cr1MoVG boiler steel pipe is used for high-pressure boilers heating surface tubes, economizer, superheater, reheater, petrochemical industrial pipe etc.
GB5310 12Cr1MoVG boiler steel pipe Chemical Composition and Mechanical Property
|
|
Steel grade |
12Cr1MoVG Chemical composition(%) |
|
||||||
|
C |
Mn |
Si |
V |
Cr |
Mo |
P |
S |
||
|
GB5310 |
12Cr1MoVG |
0.08~0.15 |
0.40~0.70 |
0.17~0.37 |
0.15-0.30 |
0.90-1.20 |
0.25~0.35 |
≤ 0.025 |
≤0.010 |
|
12Cr1MoVG Mechanical property |
||||||
|
Standard
|
Tensile strength (MPa) |
Yield strength (MPa) |
Elongation(%) |
|||
|
GB5310 |
12Cr1MoVG |
470~640 |
≥ 255 |
≥ 21 |
||
Testings
(1)Hydraulic test
The steel pipe shall be hydraulically tested one by one, and the eddy current testing can instead of the hydraulic test.
(2)Flattening test
Steel pipes with an outer diameter greater than 22 mm to 400 mm and a wall thickness not greater than 40 mm shall be subjected to a flattening test.
(3)Bending test
Steel pipes with an outer diameter greater than 400 mm or a wall
(4)Flaring test
The steel pipe with an outer diameter of not more than 76 mm and a wall thickness of not more than 8 mm can be used for the flare test.
(5)Low-power test
Steel pipes should be tested at low magnification. Visually visible white spots, inclusions, subcutaneous bubbles, tumbling and delamination are not allowed on the cross-section acid immersion test piece.
(6) Non-metallic inclusions
Steel pipes shall be tested for non-metallic inclusions.
(7)grain size
The finished steel pipe should be tested for grain size.
(8)Microstructure
The finished steel pipe will be ferrite plus pearlite, allowing the presence of granular bainite, and no phase change at critical temperature between AC1 and AC3 is allowed.
(9)Decarburization layer
Cold drawn (rolled) finished steel pipes with an outer diameter of not more than 76 mm shall be inspected for the total decarburization layer.
(10)Non-destructive testing
The steel pipe shall be ultrasonically inspected and tested in accordance with the provisions of GB/T 5777.
Boiler tube Size available: 2'to 42" SCH 40-SCH160
Pipe length: 4-12m
Packaging Details: Standard export seaworthy packing or as required.
Delivery Time: 30-50 days, 7 days for stock goods.


Galaxy Company Hot Sale Steel Pipe Products:
OCTG, casing, seamless steel pipe, line pipe, boiler tube, ASTM A333 pipe, API 5L pipe,, welded steel pipe, steel pipe inventory, Chinese pipe factory, API 5L X52 pipe, pipe fittings, tubing, API 5CT pipe, Steel pipe
You Might Also Like
-

large diameter Seamless Line Pipes API 5L GR.B 1016x25.4 mm 6 m length
-

St37 Seamless Tube 88.9mm Diameter
-

Seamless Steel Pipe ASTM A106 B NACE MR 0175 12IN SCH160
-

Seamless Line Pipe API 5L GR.B 24INCH SCH40 12M Length
-

Seamless Pipe 2inch Idimeter XXS 6 M LENGTH Export
-

Seamless Pipe ASTM A106 C 10IN Diameter XS 12M Length
Send Inquiry