GOST 550-75 15X5M Seamless Steel Boiler Pipes/Tubes
GOST 550-75 15X5M Seamless Steel Boiler Pipes are engineered for use in boiler systems and other high-temperature, high-pressure applications
Product Introduction
GOST 550-75 15X5M Seamless Steel Boiler Pipes are engineered for use in boiler systems and other high-temperature, high-pressure applications. These pipes and tubes are manufactured from carbon steel and are seamless, ensuring uniform wall thickness and superior mechanical properties.
2. Product Parameters:
| Parameter | Description |
|---|---|
| Standards | GOST 550-75 15X5M |
| Material | Carbon Steel (Seamless) |
| Size Range | Various diameters and wall thicknesses as per GOST standards |
| Length | 6-12m,Standard lengths, customizable upon request |
| Ends | Plain ends, beveled ends, threaded, or socket-weld ends |
| Surface Treatment | As-rolled, annealed, or normalized |
3. Mechanical Properties:
| Property | GOST 15X5M Requirement |
|---|---|
| Tensile Strength | ≥510 MPa (74,500 psi) |
| Yield Strength | ≥295 MPa (42,500 psi) |
| Elongation | ≥18% |
| Hardness | Varies depending on heat treatment |
4. Chemical Composition:
| Element | Typical Range (%) for 15X5M |
|---|---|
| Carbon | 0.10 - 0.16 |
| Manganese | 0.40 - 0.70 |
| Phosphorus | ≤ 0.035 |
| Sulfur | ≤ 0.035 |
| Silicon | 0.17 - 0.37 |
5. Product Uses:
- Boiler Tubes: Used for steam generation in high-pressure boilers.
- Superheater and Reheater Tubes: Employed in superheater and reheater sections of steam power plants.
- Heat Exchangers: Suitable for use in heat exchangers operating under high pressure and temperature.
- Petrochemical Industry: Utilized in pipelines and equipment within the petrochemical industry.



My company hot sale steel pipe:
ASTM A106 B seamless pipes,(1” to 24” sch40, sch80),
API 5L GR.B steel pipes, (seamless pipe, LSAW pipe, SSAW pipes, 1” to 110” sch 40, sch80),
Boiler tubes,( 20G. 12Cr1MoVG, ASTM A335 P5, P9, P11),
ASTM A333 GR.6 seamless pipes, ( 1” to 24” sch40, sch80, sch160)
My company hot sale steel pipe:
ASTM A106 B seamless pipes,(1” to 24” sch40, sch80),
API 5L GR.B steel pipes, (seamless pipe, LSAW pipe, SSAW pipes, 1” to 110” sch 40, sch80),
Boiler tubes,( 20G. 12Cr1MoVG, ASTM A335 P5, P9, P11),
ASTM A333 GR.6 seamless pipes, ( 1” to 24” sch40, sch80, sch160)
You Might Also Like
-

large diameter Seamless Line Pipes API 5L GR.B 1016x25.4 mm 6 m length
-

St37 Seamless Tube 88.9mm Diameter
-

Seamless Steel Pipe ASTM A106 B NACE MR 0175 12IN SCH160
-

Seamless Line Pipe API 5L GR.B 24INCH SCH40 12M Length
-

Seamless Pipe 2inch Idimeter XXS 6 M LENGTH Export
-

Seamless Pipe ASTM A106 C 10IN Diameter XS 12M Length
Send Inquiry