Cangzhou Galaxy Steel Pipe Co., Ltd

banner
EN 10025-3-2019 S355NL Low Alloy High Strength Steel Plate

EN 10025-3-2019 S355NL Low Alloy High Strength Steel Plate

DescriptionS355NL is a hot rolled, medium tensile, low carbon manganese steel which is readily weldable and posses

Product Introduction

Description

S355NL is a hot rolled, medium tensile, low carbon manganese steel which is readily weldable and possess good impact resistance (also in sub-zero temperatures).

This material is commonly supplied in the untreated or normalized condition and is available in several variations (denoted by additional letters and/or digits) which offer slight modifications of chemical composition and mechanical properties.

We have a large inventory of BS EN 10025-3 S355nl plate in almost all length, view S355NL Steel Plate price

S355NL Steel Plate Chemical Structure

C %

Si %

Mn %

P %

S %

V %

AL %

Cr %

0.180      

0.500      

0.9-   1.65  

0.025      

0.020         

0.120

0.020

0.300        

Cu %

Mo %

Nb %

Ni %

Ti %

N %               

                                           

0.550

0.100

0.050

0.300

0.050

0.015

   

 

Mechanical Property Of S355NL Plate

Thickness(mm)

Min Yield (Mpa)

Tensile(MPa)

Elongation(%)

Min Impact Energy

8mm-100mm

235Map-275Mpa

470-630Mpa

22%

-50

27J

101mm-200mm

285Mpa-315Mpa

450-600Mpa

21%

-50

27J

201mm-250mm

275Mpa-285Mpa

450-600Mpa

21%

-50

27J

The min impact energy is longitudinal energy

 

S355NL Structural Plates Equivalent Grades

Germany

DIN,WNr

France

AFNOR

England

BS

Italy

UNI

China

GB

Russia

GOST

TStE355

E 355 FP

50EE

Fe E 355 KT N

 

 

1. Impact Temperature

S355N: Steel plate with an impact test temperature of -20°C.

S355NL: Steel plate with an impact test temperature of -50°C.

S355ML: Steel plate with an impact test temperature of -50°C.

2. Application Fields

S355N: Mainly used in large ships, bridges, power station equipment, medium/high-pressure boilers, high-pressure vessels, railway vehicles, lifting machinery, mining machinery, and other large welded structural components.

S355NL: Commonly applied in mining machinery, chemical machinery, agricultural machinery, wind power projects, metallurgical machinery, construction machinery, road machinery, and large steel structures. In China, S355NL steel plates are mostly used for export trade or manufacturing export equipment.

S355ML: Widely used in metallurgical machinery equipment manufacturing and electromechanical equipment manufacturing. Also suitable for load-bearing parts of welded structures in low-temperature environments, such as bridges, sluices, storage tanks, and water supply tanks.

My company hot sale steel plates:

Steel plate,S355, S275, steel coil, steel sheet

 







 

You Might Also Like