SSAW Welded Line Pipe API 5L X70 PSL2 914mm Diameter 12.7mm 12m Length
Spiral Submerged- Arc Welded Steel Pipe is SSAW pipeAPI 5L SSAW Welded Line Pipe is both Applied For Oil And G
Product Introduction
Spiral Submerged- Arc Welded Steel Pipe is SSAW pipe
API 5L SSAW Welded Line Pipe is both Applied For Oil And Gas Transmissions.
It contains two product specification levels PSL1, PSL2. (Including the material for sour services uses in PSL2)
API 5L X70 PSL 1 Carbon Steel Line Pipes Chemical Composition
| Mass fraction, based upon heat and product analysis a | |||||||
| SEAMLESS PIPE | |||||||
| C | Mn | P | S | V | Nb | Ti | |
| maxb | max.b | min. | max. | max. | max. | max. | max. |
| 0.28e | 1.40e | – | 0.030 | 0.030 | f | f | f |
| WELDED PIPE | |||||||
| 0.26 | 1.45e | – | 0.030 | 0.030 | f | f | f |
API 5L X70 PSL 2 Carbon Steel Line Pipes Chemical Composition
| Mass fraction, based upon heat and product analysis % maximum | CARBON EQUIVALENT a | ||||||||||
| % MAXIMUM | |||||||||||
| Cb | Si | Mnb | P | S | V | Nb | Ti | Other | CEIIW | CEPcm | |
| SEAMLESS & WELDED PIPES | |||||||||||
| L485Q or X70Q | 0.18f | 0.45f | 1.8f | 0.025 | 0.015 | g | g | g | h | 0.43 | 0.25 |
| WELDED PIPE | |||||||||||
| L485M OR X70M | 0.12f | 0.45f | 1.7f | 0.025 | 0.015 | g | g | g | h | 0.43f | 0.25 |
API 5L X70 PSL 1 Carbon Steel Line Pipes Mechanical Properties
| Y.S | T.S | ELONGATION |
| Mpa(psi) | Mpa(psi) | |
| min | min | min |
| 485(70 300) | 570(82 700) | F |
API 5L X70 PSL 2 Carbon Steel Line Pipes Mechanical Properties
| Y.S | T.S | ELONGATION |
| Mpa(psi) | Mpa(psi) | |
| min-max | min-max | min |
| 485(70 300)-635(92100) | 570(82700)-760(110200) | F |
•0.50% maximum for copper, 0.50% maximum for nickel, 0.50% maximum for chromium, and 0.15% maximum for molybdenum.
• For each reduction of 0.01% below the specified maximum concetration for carbon, an increase of 0.05% above the specified maximum concentration for manganese is permissible, up to a maximum of 1.65%
• Unless otherwise agreed, the sum of the niobium and vanadium contents shall be ≤0.06%.
• The sum of the niobium ,vanadium and titanium concentratons shall be ≤0.06%.
• Unless otheriwse agreed.
• Unless otherwise agreed, the sum of niobium, vanadium and titanium concentrations shall be ≤ 0.15%

Our Supply Range For API 5L SSAW Welded Pipe
Grades: API 5L Grade B, X42, X52, X56, X60, X65, X70, X80
Product Specification Level: PSL1, PSL2, onshore and offshore sour services
Size: 8"-110"
Wallthickness: 6-25.4mm
Ends Type: Beveled ends, Plain ends
Length Range: SRL (Single Random Length), DRL (Double Random Length)
Protection Caps in plastic or iron
Surface Treatment: Natural, Varnished, Black painting, FBE, 3PE (3LPE), 3PP, CWC (Concrete Weight Coated) CRA Clad or Lined

Galaxy Company Hot Sale Steel Pipe Products:
OCTG, casing, tubing, seamless steel pipe, line pipe, boiler tube, ASTM A333 pipe, ASTM A335 alloy pipes, API 5L pipe,, welded steel pipe,LSAW pipes, steel pipe inventory, Chinese pipe factory, API 5L X52 pipe, pipe fittings, API 5CT pipe, Steel pipe, stainless steel pipes.
You Might Also Like
-

large diameter Seamless Line Pipes API 5L GR.B 1016x25.4 mm 6 m length
-

St37 Seamless Tube 88.9mm Diameter
-

Seamless Steel Pipe ASTM A106 B NACE MR 0175 12IN SCH160
-

Seamless Line Pipe API 5L GR.B 24INCH SCH40 12M Length
-

Seamless Pipe 2inch Idimeter XXS 6 M LENGTH Export
-

Seamless Pipe ASTM A106 C 10IN Diameter XS 12M Length
Send Inquiry