Seamless Line Pipe API 5L X42 PSL1 14" XS 6m length
Stock ofAPI 5L seamless line pipeCangzhou Galaxy Companyisone of the leading supplier stockiest & exporter of high
Product Introduction
Stock of API 5L seamless line pipe
Cangzhou Galaxy Company is one of the leading supplier stockiest & exporter of high quality API 5L Seamless Steel Pipes and alloy tubes,
Carbon steel is more commonly used than any other metal, and has long been admired for its versatility and low cost. As a specialist in scheduled and non-scheduled wallthickness seamless pipe and tube, Galaxy Steel supply stocks a complete size range of seamless carbon steel pipe and tube. We offer multiple grades of carbon steel covered by ASTM A106, ASME A 53 and API specifications:
API 5L is the specification for line pipe. This carbon steel pipe is used for pipeline transportation systems. Our API 5L seamless line pipe is only manufactured from premium mills of china in a variety of grades; B, X42, X52, X60, X65, X70 and X80 in both PSL-1 and PSL-2
API 5L GR. B PSL 1 Seamless Pipes:
| CHEMICAL COMPOSITION | ||||||
| Mass fraction, based upon heat and product analysis a | ||||||
| SEAMLESS PIPE | ||||||
| C | Mn | P | V | Nb | Ti | |
| maxb | max | max. | max. | max. | max. | max. |
| 0.28 | 1.20 | 0.030 | 0.030 | c,d | c,d | d |
| WELDED PIPE | ||||||
| 0.26 | 1.20 | 0.030 | 0.030 | c,d | c,d | d |
| MECHANICAL REQUIREMENTS | ||
| Y.S | T.S | ELONGATION |
| Mpa(psi) | Mpa(psi) | |
| min | min | min |
| 245(35 500) | 415(60 200) | 28% |
API 5L X42 PSL1 Seamless Line Pipe
Chemical Composition
|
Grade |
C (Max) |
Si (Max) |
Mn (Max) |
P (Max) |
S (Max) |
Cr (Max) |
Cu (Max) |
Mo (Max) |
V (Max) |
|
X42 PSL 1 |
0.22 |
0.45 |
1.3 |
0.025 |
0.015 |
0.4 |
0.4 |
0.15 |
0.05 |
Mechanical Properties
|
API 5L Grade |
Yield Strength |
Tensile Strength |
Elongation |
|
X42 PSL 1 |
290~495 |
415~760 |
23 |
Galaxy Steel Offers A Wide Range Of API 5L B, X42, X52, X60, X70 PSL-1 & PSL-2 Line Pipe In Seamless & SSAW Steel Pipeline. API 5L Carbon Steel Seamless Pipes Are Available In Size Range Of 1/2” NB Through 36”, Welded API 5L Carbon Steel Pipes Are Available In Large Diameter To 3000mm. The stock is available for above pipes.


Galaxy Company Hot Sale Seamless Steel Pipe Products:
seamless steel pipe, line pipe, ASTM A106 pipe, , Mechanical pipe, API 5L pipe, boiler tube,ASTM A335 alloy pipes,GB/T5310 boiler Tub
You Might Also Like
-

large diameter Seamless Line Pipes API 5L GR.B 1016x25.4 mm 6 m length
-

St37 Seamless Tube 88.9mm Diameter
-

Seamless Steel Pipe ASTM A106 B NACE MR 0175 12IN SCH160
-

Seamless Line Pipe API 5L GR.B 24INCH SCH40 12M Length
-

Seamless Pipe 2inch Idimeter XXS 6 M LENGTH Export
-

Seamless Pipe ASTM A106 C 10IN Diameter XS 12M Length
Send Inquiry