Cangzhou Galaxy Steel Pipe Co., Ltd

banner
EN10297-1 E355 seamless steel pipe  508x65  8-12m length

EN10297-1 E355 seamless steel pipe 508x65 8-12m length

EN10297-1 E355 seamless steel pipeEN10297-1 E355 seamless steel pipes are mainly used for hydraulic, pneumatic cyli

Product Introduction

EN10297-1 E355 seamless steel pipe

EN10297-1 E355 seamless steel pipes are mainly used for hydraulic, pneumatic cylinder, hydraulic lines, spinning, textile and printing machinery pipe, automobile shock absorber tube, sleeve tube, rod and precision machinery with steel.

The code E355 points to certain mechanical characteristics such as a minimum yield strength of 355 MPa and improved ductility for use in high pressure and at different temperatures. The most important feature of E355 seamless pipes is that they are seamless, which means that they offer consistent and dependable performance. Seamless pipes are made through a process of making a round steel billet which is then pierced to make a round pipe without any welds. This method reduces some of the flaws usually found in welded pipes, thus increasing their capacity to handle internal pressures and stress. Therefore, E355 seamless pipes are used in applications where leakage or failure can be disastrous in the operation of the equipment.

These pipes are widely used in oil and gas exploration, petrochemicals, automobile, mechanical engineering, and construction industries. They are useful in the transport of various fluids and gases at high pressures such as water, oil, gases, and chemicals. The smooth surface of E355 pipes also makes it easier to install and maintain, thus cutting down on time and expenses for the end-users.

E355 seamless pipes have good machinability and weldability, which makes the pipes easy to process and adapt to the needs of a particular project. Their mechanical properties are uniform and reliable, which makes them reliable in applications where performance is critical and where engineers and designers need to be assured of the material’s performance.

EN10297-1 E355 seamless steel pipe Chemical composition %

C 

Si

Mn              

P       

S

max   0.22

max   0.55

max   1.6

max   0.030

max   0.035

EN10297-1 E355 seamless steel pipe mechanical properties:

Yield strength     

Tensile strength            

Elongation        

≥ 295 MPa

≥470 MPa

≥ 18

 

My company hot sale seamless steel pipes:

ASTM A106 B seamless pipes,(1” to 24” sch40, sch80),

API 5L GR.B steel pipes, (seamless pipe, 1” to 30” sch 40, sch80),

Boiler tubes,( 20G. 12Cr1MoVG, ASTM A335 P5, P9, P11),

ASTM A333 GR.6 seamless pipes, ( 1” to 24” sch40, sch80, sch160),

API 5CT seamless casing, and tubing, (2 3/8” to 20” K55, J55, N80, L80, P110),