ASTM A671 Grade CC70  LSAW welded pipe 28" sch80  12m length

ASTM A671 Grade CC70 LSAW welded pipe 28" sch80 12m length

ASTM A671 Grade CC70is standard Specification utilized for Electric Fusion Welded Steel Pipe for Atmospheric and L

Product Introduction

ASTM A671 Grade CC70 is standard Specification utilized for Electric Fusion Welded Steel Pipe for Atmospheric and Lower Temperatures reason. A671 CC 70 Pipes are created from weight vessel quality plate of various investigation and quality dimensions and proper for high-weight administration at barometrical and lower temp.

ASTM A671 CC70 specification covers standard requirements for electric-fusion-welded steel pipe with filler metal added, for atmospheric and lower temperatures. The steel pipe shall be fabricated from a pressure vessel quality plate of several analysis and strength levels. Several grades and classes of pipe shall be provided. Grade shall designate the type of plate used while class shall designate the type of heat treatment performed during pipe manufacture. Class shall be designated as to whether the weld is radiographically examined, and as to whether the pipe is pressure tested. Steel samples shall undergo tension and transverse guided weld bend tests and conform to the specified mechanical requirements.+

Carbon Steel A671 CC70 - Characteristics

ASTM A671 Pipe is made up of pressure vessel plates that are suitable for service at elevated temperatures as well as at lower temperatures.  A671 CC70 CL22 EFW Pipe may or may not be treated with heat to attain the desired property. Though the cost of ASTM A671 Gr CC70 Welded pipe is low they offer a variety of properties. 

  • Low-temperature services serve at -45F°F (-45°C)
  • Excellent strength and ductility
  • Better weldability and greater toughness
  • Higher strength with low coefficients of thermal conductivity than alloy steels

Looking for A671 CC60, CC65, CC70 Pipe Supplier 

A671 CC70 Pipe Chemical Compostion and Mechanical Properties

Specification Steel grade C Si Mn P S Ti Remarks
Pipes for pressure service
ASTM A671, A672
-/A45 -/0.17 – 0.98 0.035 0.035 – A671/
A672
-/A50 -/0.22 –
CA55/A55 0.28 –
-/B55 -/0.20 0.13
~0.45
CB60/B60 0.24
CB65/B65 0.28
CB70/C70 0.31 1.30
-/C55 -/0.18 0.55
~0.98
CC60/C60 0.21
CC65/C65 0.24 0.79
~1.30
CC70/C70 0.27
Products Steel Grade Base Metal Mechanical Composition Welding point tensile strength (N/mm2) Remarks
Yield point (N/mm2) Tensile Stregth (N/mm2) Test Pcs Elongation (%)
Pipes for pressure service ASTM A671, A672 -/A45 -/165 -/310~450 – -/30 -/310~450 A671/ A672
-/A50 -/185 -/345~485 -/28 -/345~485
CA55/A55 205 380~515 27 380~515
-/B55 -/205 -/380~515 -/27 -/380~515
CB60/B60 220 415~550 25 415~550
CB65/B65 240 450~585 23 450~585
CB70/B70 260 485~620 21 485~620
-/C55 -/205 -/380~515 -/27 -/380~515
CC60/C60 220 415~550 25 415~550
CC65/C65 240 450~585 23 450~585
CC70/C70 260 485~620 21 485~620




 

Hot Tags:

stainless pipe a312 gr.tp304l, EFW pipe,36.19,sch.10s 18in, pipe suppliers, factory, cheap price, discount, bulk, customized, astm a335 p11 alloy seamless pipe, astm a106 b seamless pipe, astm a335 p22 alloy seamless pipe, SSAW pipes diameter 711mm, structure seamless pipe, astm a671 gr lsaw welded pipes